Description
Precautions
01. Thoroughly clean the bonding surfaces before application. Make sure the substrates are clean and free of contaminants for a secure bond.
02. Control the application temperature carefully. Prolonged operation above 180°C may cause adhesive degradation and reduce bonding strength.
03.Open time and curing performance may vary with adhesive temperature, ambient temperature, coating amount, bonding time, and pressure. Adjust the application conditions as needed.
04. Keep the product out of reach of children. Molten adhesive is extremely hot. Do not touch it during operation to avoid burns.
05. In case of a burn, immediately immerse the affected area in cool water for at least 10 minutes and seek medical attention. For complete safety information, refer to the product MSDS.
Key Benefits
01.100% Solids and Solvent-Free for Cleaner Production
With 100% solids content and a solvent-free formulation, OGD-A6090 features low odor and no irritating volatile substances, supporting the cleanliness and environmental requirements of hygiene product manufacturing.
02.High Cohesive Strength for Reliable Lamination
Excellent cohesive strength provides strong bonding between nonwoven fabrics and PE films, helping prevent delamination and peeling under stretching, compression, and daily use conditions.
03.Excellent Melt Flow for High-Speed Production Lines
The adhesive melts smoothly and evenly, providing stable adhesive output and reliable processing performance for automated high-speed hygiene product lamination lines, improving production efficiency.
04.Optimized for Hygiene Material Substrates
The formulation is specially optimized for nonwoven fabrics and PE films, providing balanced initial tack and final adhesion to help solve common bonding failure issues in hygiene material applications.
05.Easy Process Management with Stable Performance
Following the first-in, first-out (FIFO) storage principle helps maintain consistent adhesive performance over time. Simple process control supports stable production and improves finished-product yield.